WEKO3
アイテム
木材の老化に関する研究 第 XVI 報 : 古材及び熱処理材における組成の変化の比較(その 1)
https://kpu.repo.nii.ac.jp/records/5681
https://kpu.repo.nii.ac.jp/records/56816e53853f-6c4f-4b79-b09d-15e3acde12c1
名前 / ファイル | ライセンス | アクション |
---|---|---|
![]() |
|
Item type | [ELS]紀要論文 / Departmental Bulletin Paper(1) | |||||||||||||||||||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
公開日 | 2017-02-20 | |||||||||||||||||||||||||||||
タイトル | ||||||||||||||||||||||||||||||
タイトル | 木材の老化に関する研究 第 XVI 報 : 古材及び熱処理材における組成の変化の比較(その 1) | |||||||||||||||||||||||||||||
言語 | ja | |||||||||||||||||||||||||||||
その他(別言語等) | ||||||||||||||||||||||||||||||
その他のタイトル | Studies on the permanence of wood (XVI) : Analysis of heat treated wood compared with old timbers (Part 1) | |||||||||||||||||||||||||||||
言語 | en | |||||||||||||||||||||||||||||
言語 | ||||||||||||||||||||||||||||||
言語 | jpn | |||||||||||||||||||||||||||||
資源タイプ | ||||||||||||||||||||||||||||||
資源タイプ | departmental bulletin paper | |||||||||||||||||||||||||||||
著者 |
小原, 二郎
× 小原, 二郎
× 岡本, 一
× 重松, 頼生
|
|||||||||||||||||||||||||||||
抄録(英) | ||||||||||||||||||||||||||||||
内容記述タイプ | Other | |||||||||||||||||||||||||||||
内容記述 | Oven dryed saw dust of HINOKI (Chamaecyparis obtuse ENDLICHER) and that of KEYAKI (Zelkowa serrata MAKINO) are analysed at intervals of 4days. The temperature of heating is 130℃, during 12days. From the results of the analyses (Table 1 and Fig. 1), the rate of increase or decrease of content of each constituent is calculated (Table 2), and compared with the data on the corresponding old timbers (Fig. 2). The conclusions obtained from this comparison are as follows : 1) The difference between the rate of decomposition of cellulose in KEYAKI and the rate in HINOKI, which is evident in the old timbers, becomes less significant under this condition (Fig. 2). 2) In this heat treatment, the amount of generated soluble constituents, accompanied with the decomposition of the standard amount of cellulose, is less than that amount found in the old timbers (Table 3). And with KEYAKI the amount is less than with HINOKI (Fig. 2). 3) The rate of decomposition of cellulose under this condition is about (10)^4∿(10)^5 times as much as the rate in the old timbers (Table 4). | |||||||||||||||||||||||||||||
言語 | en | |||||||||||||||||||||||||||||
書誌情報 |
ja : 西京大学学術報告. 農学 en : The scientific reports of the Saikyo University. Agriculture 巻 7, p. 57-61, 発行日 1955-09-01 |
|||||||||||||||||||||||||||||
雑誌書誌ID | ||||||||||||||||||||||||||||||
収録物識別子タイプ | NCID | |||||||||||||||||||||||||||||
収録物識別子 | AN00094635 | |||||||||||||||||||||||||||||
ISSN | ||||||||||||||||||||||||||||||
収録物識別子タイプ | PISSN | |||||||||||||||||||||||||||||
収録物識別子 | 03709329 |